External masonry walls: assessing whether cracks indicate progressive movement.

External masonry walls: assessing whether cracks indicate progressive movement. - Garston, Watford Building Research Establishment 1987 - 1 sheet: ill. ; 30cm. - Defect Action Sheet 102 (Design) DAS 102 .